Key Takeaways
- Most cracks in a concrete factory floor are shrinkage cracks: concrete shrinks as it dries and cracks wherever something holds it back, such as columns, pits, joints set too far apart or racking loaded too early. They are usually non-structural. Cracks with sunken areas, stepped edges, gaps at the walls or jamming shutters point to settlement and need an engineer.
- Movement matters more than width. A stable 2 mm crack may be insignificant, while one widening by 1 mm a month is very significant. Measure and date the cracks before you sign, and ask when they first appeared.
- A weak floor can usually be strengthened (thicker pads under machines, grout under the slab, micropiles on soft ground, bonded fibre strips under upper floors), but it is a structural alteration: a Professional Engineer designs it and the council's written permission comes first.
- Heavy presses and other machines with strong impact or vibration usually need their own reinforced concrete foundation, separate from the floor, designed from the manufacturer's loads. Selangor's by-laws require at least a 20% allowance for machine impact and vibration, and the DOE guideline recommends vibration limits at the neighbours.
- No law makes epoxy compulsory in every factory. It becomes necessary in effect where a rule asks for an impervious, washable or crack-free floor, such as food premises under the Food Hygiene Regulations 2009 and scheduled waste stores under the DOE guideline. Epoxy laid over a damp or moving slab blisters and cracks.
A cracked or sinking floor can stop racking, forklifts and machines, and it is expensive to fix once you have moved in. This guide explains why factory floors crack and settle, how to tell a harmless crack from a warning sign, how to check a used factory floor before you buy or rent, what can be done to strengthen a floor or repair settlement, what a foundation for a heavy machine or large press involves, and when an epoxy floor is really needed. For design loads in kN/m² and racking checks, read our guide to factory floor loading first. This guide explains rules and engineering practice in general terms and is not engineering or legal advice: a Professional Engineer must assess your floor.
Why does a factory floor crack?
Concrete shrinks as it dries and cracks wherever it is restrained. Most other cracks come from loads the floor was not designed for, or from the ground moving underneath. The first group is common and usually harmless; the last group is the one that costs money.
Shrinkage and restraint cracks
The Association of Concrete Industrial Flooring Contractors (ACIFC) puts it plainly in its technical note on cracks in industrial concrete floors: shrinkage cracks do not form unless there is some restraint, and they form when the tensile stress exceeds the tensile strength of the concrete. The typical non-structural cracks it lists are:
- Re-entrant corner cracks running from the corners of columns, pits, walls and office blocks, where the shrinking slab is held back.
- Mid-panel and mid-aisle cracks, often from joints placed too far apart, or from racking installed and loaded soon after the floor was cast.
- Cracks over ruts in the sub-base, where the slab ended up thinner than designed.
- Cracks where the slab changes depth without a joint between the two areas.
- Cracks parallel to construction joints, where misaligned dowels lock the joint.
- Cracks around base plates drilled in later for a mezzanine or new machines, especially within about two years of casting.
ACIFC adds that a joint is essentially a planned crack, and that a non-structural crack that stays within the specified tolerances needs no repair.
Curling at the joints
A slab curls when its top dries and shrinks faster than its bottom, lifting the edges and corners. The National Ready Mixed Concrete Association's guide to curling explains that curling leaves part of the slab unsupported, which can lead to cracking under heavy loads and to chipped and spalled joint edges under traffic. Poor curing, slabs cast straight onto plastic sheeting, thin slabs and long joint spacing make it worse. If forklift wheels bang at the joints or a panel rocks underfoot, suspect curling.
Cracks from loads and vibration
Heavier racking and machines than the floor was designed for, and vibration, also crack floors. Selangor's building by-laws require concentrated loads from installed machinery, including impact and vibration, to be provided for in the design, with an increase of at least 20% (by-law 68 of the Selangor Uniform Building By-Laws). A floor designed for storage has no such allowance in the spot where you later put a press.
Piled floors are a different case
Some factory slabs, especially on soft ground, are carried on piles. ACIFC warns that a piled floor is suspended between the piles and acts as a structure, so its cracks should not automatically be treated as non-structural. A grid of cracks mirroring the pile positions below is a known pattern, and the most common failure mode is bending over the piles. Cracks in a piled slab call for an engineer.
Settlement of the ground
When the fill or soil under a ground-bearing slab compresses or washes out, the slab loses support and cracks, sinks or steps. The Concrete Society notes that a ground-supported floor only works on ground that will not let the slab settle excessively.
| What you see | Likely cause | Usually serious? |
|---|---|---|
| Fine, shallow surface cracks that appeared soon after casting | Early shrinkage | Rarely |
| A straight crack across a panel between joints | Drying shrinkage, joints too far apart, early racking | Usually not, if within tolerance |
| Cracks from the corners of columns, pits or walls | Re-entrant corner restraint | Usually not |
| Lifted or rocking slab edges, broken joint edges | Curling | Affects forklifts; repairable |
| Cracks radiating from machine bases or drilled anchors | Loads or vibration the floor was not designed for | Depends on the design: check |
| A grid of cracks over pile positions | Piled slab bending over the piles | Treat as possibly structural |
| Sunken bays, stepped cracks, gaps under walls | Settlement of the fill or soft ground | Yes, until shown to have stopped |
What are the signs of settlement in a factory?
Settlement shows as floors that slope or pond water, sunken bays near doors and drains, cracks with one side lower than the other, gaps between the floor and the walls, and doors and roller shutters that start to jam. In walls, the classic pattern is diagonal, stepped cracking that tapers and is wider at the top, running through door and window openings.
What engineers look for
The Subsidence Forum's seminar notes on structural movement in buildings list the questions to ask: is the cracking diagonal, vertical or horizontal; does it taper; are bed joints, sills and floors level; are the walls plumb; are door and window frames square; and have repairs already been done? Its notes on subsidence add:
- Diagonal stepped cracks, wider at the top, run through weak points such as door and window openings.
- Extensions can rotate away from the main building because their foundations differ, leaving tapering cracks at the junction. Factories with a later rear extension or canopy are worth a close look here.
- Cracks in clay ground may open and close as the soil wets and dries.
- In terrace and semi-detached buildings, neighbouring units of similar construction may show the same defect, which points to a shared cause.
How wide is too wide?
For wall cracks, engineers use the BRE Digest 251 damage categories, reproduced in the same notes:
| Category | Typical crack width | What it means |
|---|---|---|
| 0 | Hairline, about 0.1 mm | No action needed |
| 1 | Up to 1 mm | Treated in normal decoration |
| 2 | Up to 5 mm | Easily filled; doors and windows may stick slightly |
| 3 | 5 to 15 mm | Opening up and patching; doors and windows stick; pipes may fracture |
| 4 | 15 to 25 mm | Sections of wall replaced; frames distorted; floor sloping noticeably |
| 5 | Over 25 mm | Major repair or rebuilding; beams lose bearing; walls need shoring |
What matters most is whether the movement is progressive: a stable 2 mm crack may be dismissed as insignificant, but one increasing by 1 mm a month is very significant. Where in doubt, crack or level monitoring is the next step.
Why soft ground in Klang matters
G&P Geotechnics, a Malaysian geotechnical consultancy, describes in a paper on geotechnical practice in Malaysia how development has spread onto very soft alluvial soils and marine clays, where the stiff layer and bedrock can be very deep, sometimes more than 60 m. Works on deep soft clay are associated with excessive differential settlement, negative skin friction (settling soil dragging down on piles) and bearing failure. At Bukit Tinggi in Klang, the paper shows 25 to 30 m of very soft to medium stiff silty clay, known as Klang Clay, over dense sand. It names two more triggers: former mining land, where slime ponds and loose fill can go on settling, and groundwater lowered by nearby excavation, which caused cracks and settlement in surrounding buildings over a zone up to 30 times the excavation depth. In Klang, Kapar and Port Klang, ask whether the slab sits on the ground or on piles, and ask for the soil investigation. For Pulau Indah, a partner site has a guide to piling and settlement checks on soft ground.
How do you check a used factory floor before buying or renting?
Read the drawings, ask for the history, walk and measure the floor, then have a Professional Engineer test what you cannot see. Do it before you sign, and make the result a condition of the deal.
- Ask for the documents. The approved building and structural plans (Selangor's by-law 16(3) requires each floor's design load to be marked on them), the Certificate of Completion and Compliance, approved plans for any mezzanine or extension, the soil investigation report and records of past floor repairs. Since the 2012 amendment, by-law 73 has required foundations to be designed from a proper site investigation supervised by a Professional Engineer with geotechnical experience, so a building approved since then should have one.
- Ask for the history. When were the cracks first noticed, have they changed, what was repaired and when, has the site flooded, and where did heavy machines and racking stand? Cracks running through fresh paint, filler or a new coating point to recent movement.
- Walk the whole floor. Use the checklist below, and look under racking and behind stock, where problems hide.
- Measure and record. Crack widths with a crack gauge, dated photos, and a level survey across the bays if anything looks sunken. If there is time before signing, fix tell-tale monitors across the key cracks and read them again.
- Bring in a Professional Engineer. Section 85A of the Street, Drainage and Building Act 1974 sets out what a full structural investigation involves: checking the structural plans and calculations (or reconstructing them), non-destructive tests on structural elements, tests on building materials and load tests where needed. The section applies to buildings over five storeys, but the same steps are the template for a serious floor check.
- Write it into the deal. For a purchase, make a satisfactory engineer's report or agreed repairs a condition in the offer letter and the SPA. For a lease, record the floor's condition with photos at handover and agree who fixes what (see who is responsible for factory repairs).
| Where to look | What to check | What it can mean |
|---|---|---|
| Joints | Lifted edges, spalling, rocking panels, sealant squeezed out | Curling, loss of support |
| Columns, pits, drains, dock levellers | Cracks from the corners, sunken edges | Restraint, washout near drains |
| Floor to wall junction | Gaps, stepped skirting, cracks in the wall above | Settlement |
| Doors and roller shutters | Jamming, uneven gaps | Movement of the frame or floor |
| Machine bases and old anchor holes | Cracks radiating from bases, patched pits | Past heavy loads, vibration |
| Loading apron and driveway | Sinking, ponding | Settlement and drainage |
| Repaired areas | New screed, fresh coating, patched strips | What was hidden, and why |
| Units next door (terrace, semi-D) | The same cracks next door | Shared ground or construction defect |
Can a weak factory floor be strengthened, and can settlement be repaired?
Yes in most cases. First find out why the floor failed and whether the ground is still moving, because a repair on moving ground fails again. ACIFC adds that early repair of non-structural cracks may be unwise because the concrete is still shrinking: aim for one repair, not several.
Repair or alteration, and the approvals
Selangor's by-laws apply the load rules to structural alterations and additions and to existing construction on a change of use, but not to maintenance or replacing parts where the use does not change (by-law 55). In practice, patching cracks and resealing joints is maintenance, while making a floor carry presses or racking it was not designed for is an alteration that must be designed for the new loads. Under section 70(11) of the Street, Drainage and Building Act, altering a building without the council's prior written permission is an offence, and a Magistrate's Court can order the building altered or demolished. Councils may accept a sketch plan and permit for minor works (by-law 18). A tenant also needs the landlord's written consent and should agree at the start what happens to the work at the end of the lease.
Common methods
| Problem | Method an engineer may propose | Point to note |
|---|---|---|
| Voids under the slab, rocking or curled panels | Grout injected under the slab; curled joints ground level | Both listed by NRMCA as repairs for curling |
| Slab sound but too weak where machines or rack legs stand | Cut out and recast thicker, reinforced pads or strips, separated from the old slab by joints | ACIFC: separate different slab depths with a joint |
| Ground still settling under part of the building | Underpin with micropiles down to firmer strata | Micropiles are a common remedial option in Malaysia |
| Suspended upper floor too weak | Fibre reinforced polymer (FRP) strips or grids bonded to the slab soffit, or added steel members | Repair the concrete before strengthening |
| Surface worn or cracked but structurally sound | New topping or resin screed | Cracks in the slab reflect through a thin finish |
A G&P paper on micropiles describes them as widely recognised in Malaysia as a common remedial option for underpinning structures with foundation problems, in sizes from 100 mm to 350 mm carrying 150 kN to 2,800 kN. The US Federal Highway Administration's report on strengthening techniques notes that bonded FRP can strengthen one-way and two-way concrete slabs when applied to the slab soffit, after the concrete has been repaired. On deep soft clay, piles are not a simple cure: G&P notes that negative skin friction reduces pile capacity over time, so the design needs geotechnical input.
Costs vary widely with the cause, the area, the method and whether the factory keeps running during the works. Ask for an engineer's repair scheme first, then compare quotes priced on that same scheme.
Ground floor or upper floor?
The ground floor of most factories is a slab on the ground or on piles; the upper floors of terrace and semi-detached factories are suspended slabs, often designed for office loads. Strengthening a ground slab is mostly about what is underneath it; strengthening an upper floor is about the slab, beams and columns, and the extra load still has to travel down to the foundations. Work out the tonnes per square metre you need with the floor loading calculator before you brief the engineer.
What foundation does a heavy machine or large press need?
A press, forging hammer, large compressor or other machine with strong impact or vibration usually needs its own reinforced concrete foundation, separated from the surrounding floor and designed by a Professional Engineer from the manufacturer's data. Whether a lighter machine can stand on the existing slab depends on its weight, foot size and vibration measured against the slab's design.
Why the slab alone is often not enough
In the 28th ISET Annual Lecture on foundations for industrial machines, K.G. Bhatia writes that all machine foundations, whatever the size and type of machine, should be treated as engineering problems, and that complete knowledge of how the machine transfers its load and of its exciting forces and frequencies is a must. Foundations are usually solid blocks or frames of reinforced concrete. Where isolators are used, the machine sits on an inertia block made heavy enough, with a mass two to three times that of the machine, to keep the system stable. The DOE's Guidelines for Environmental Vibration Limits and Control gives the same practical rule: machinery generating high vibration should be supported on stiff structural supports with vibration isolators on inertia blocks.
Rules that apply in Selangor
- Impact and vibration (by-law 68): dynamic loads from machinery must be allowed for, with an increase of not less than 20% or the MS EN 1991-1-1 minimum, whichever is higher. Loads while equipment is being installed or moved must also be provided for, which includes the route the press takes across the floor.
- Foundations (by-law 73): foundations must be designed from a proper site investigation and must not cause settlement beyond the design limits or damage the building or any adjoining building.
- Near drains (by-law 78): within a distance from a drain at least equal to its depth, the foundation level must be at least 450 mm below the drain invert, unless the whole building is on piles.
- Party walls (by-law 79): where a wall stands against a party wall, its concrete foundations must not extend beyond your own lot boundary, which limits large bases in terrace and semi-detached factories.
- Permission (section 70 of the Act): a new foundation or pit is building work. Get the council's permission and, as a tenant, the landlord's written consent.
Vibration and the neighbours
The DOE guideline names power presses as a source of intermittent vibration and recommends limits measured at the receiving building. For intermittent vibration it recommends 3.2 mm/s for industrial receivers day and night, 1.6 mm/s for commercial and business premises, and 0.8 to 1.6 mm/s by day and 0.4 mm/s at night for homes. A press in a factory that borders shophouses or housing therefore needs more care than one in the middle of an industrial estate. The guideline also notes that distance between the source and the receiver is one of the most effective ways to cut vibration.
Installing a large press, step by step
- Get the manufacturer's foundation drawing and data: weight, centre of gravity, dynamic forces, stroke rate, anchor bolt layout and any pit depth.
- Check the unit: floor type (ground-bearing or piled), soil report, groundwater, drains and party walls near the planned spot, and crane access or headroom for installation.
- Appoint a Professional Engineer to design the foundation, its isolation from the surrounding slab, any isolators and the route in.
- Get council permission and the landlord's consent, and agree what happens to the foundation at the end of a lease.
- Build, and let the concrete reach the strength the engineer specifies before the press is set and grouted.
- After commissioning, measure vibration at the boundary if neighbours are close.
For the other specs a press shop needs, such as power, crane capacity and height, see metal fabrication factory requirements.
Is epoxy coating needed on a factory floor?
No law requires epoxy in every factory. It is needed in effect where a rule or a customer audit calls for an impervious, washable, crack-free or static-controlled floor, or where chemicals, hygiene or dust matter. In a dry storage warehouse the choice is about dust, wear and cleaning, and the right system depends on the traffic.
When a rule effectively requires a sealed floor
| Use | Rule | What the floor must be |
|---|---|---|
| Food factories and food warehouses | Food Hygiene Regulations 2009, regulation 18 | Maintained in good condition, easily cleaned, of impervious, non-absorbent, washable and non-toxic materials unless the health authority accepts another material, and adequately drained; wall to floor angles sealed and coved where necessary (regulation 19) |
| Scheduled waste store | DOE Guidelines for Packaging, Labelling and Storage of Scheduled Wastes | Floor of the store and its loading area covered with concrete or a suitable lining, free of cracks and gaps; a dike holding 110% of the container with the greatest capacity, graded to a sump |
| Static-sensitive electronics | Customer and process specifications | Static-controlled resin grades exist in FeRFA types 3 to 8 |
| Chemical handling | The chemicals actually used | Selected resins resist many chemicals; thin types 1 to 3 are not generally recommended for spillage |
The food rule is wider than restaurants: the Food Act 1983 defines food premises as premises used for or in connection with the preparation, preservation, packaging, storage, conveyance, distribution or sale of any food. Epoxy and polyurethane systems are common ways to meet regulation 18, but the regulation sets the standard, not the product. More on fit-out for food plants: food processing factory requirements.
Which system: the FeRFA types
The Resin Flooring Association (FeRFA) classifies resin floors by thickness and duty in its guide to synthetic resin flooring:
| Type | Name | Typical thickness | Duty |
|---|---|---|---|
| 1 | Floor seal | Up to 150 µm | Light |
| 2 | Floor coating | 150 to 300 µm | Light to medium |
| 3 | High build floor coating | 300 to 1,000 µm | Medium |
| 4 | Multi-layer flooring | Over 2 mm | Medium to heavy |
| 5 | Flow applied (self-smoothing) | 2 to 3 mm | Medium to heavy |
| 6 | Resin screed | Over 4 mm | Medium to heavy |
| 7 | Heavy duty flowable | 4 to 6 mm | Heavy to very heavy |
| 8 | Heavy duty resin flooring | Over 6 mm | Very heavy |
FeRFA says types 1 to 3 are generally suitable only for pedestrian, commercial or lighter industrial use; where there is regular or heavy forklift traffic, types 4 and above are most suitable, and types 7 and 8 for the heaviest use with impact. It also warns that thin coatings can fail early where grit or metal swarf is ground into the surface by traffic, which matters in machining and fabrication shops. When you compare quotes, ask each contractor to state the FeRFA type and thickness, so you compare like with like.
Why epoxy floors fail
- Cracks and joints underneath. FeRFA states that the resin is only a protective finish, the slab must be designed on its own to carry the loads, cracking of the substrate is likely to reflect in the finish, and all live movement joints must be carried through the resin. Coating over a moving crack does not stop it.
- Moisture. Unless the manufacturer says otherwise, the slab surface should have a relative humidity of not more than 75% (BS 8203 test), and a 150 mm slab can take more than a year to dry from one face. Ground slabs should have a damp proof membrane; where an existing slab has none, FeRFA lists a new membrane with an unbonded screed, a surface membrane or a moisture tolerant resin. Separately, osmotic blisters can appear in thin systems up to about 6 mm thick between three months and two years after laying.
- A weak surface. FeRFA asks for rebound hammer readings generally above 25, or a pull-off strength normally above 1.5 N/mm².
- Heat. Most resins soften at 50 to 100°C and should not be exposed directly to temperatures above 100°C, which matters near furnaces, ovens and hot work.
- Too little curing time. FeRFA gives typical cures of 1 to 3 days before significant traffic and 3 to 7 days before wet cleaning, chemicals or heavy traffic, at 15 to 20°C; follow the manufacturer's figures for site conditions.
Costs vary with the type, thickness, preparation and crack repair, so price per square metre only against an agreed specification. In a rented unit, agree with the landlord whether the coating stays or must be removed at the end of the lease.
Common mistakes
- Coating or tiling over cracks before finding out whether they are still moving.
- Treating every crack as a disaster, or every crack as cosmetic: the pattern and the movement decide.
- Bolting a press or hammer straight onto a slab designed for storage.
- Loading racking onto a new slab in its first weeks without checking with the floor contractor.
- Accepting "the cracks have always been there" without measuring them.
- Building machine bases or pits without council permission and landlord consent, which can surface at licence renewal, insurance or sale.
Mezzanine approval, overhead cranes, clear height and a full building inspection of a used factory are separate topics with their own guides; this one stays with the floor.
Practical steps: more questions
Can I install a large press in a terrace or semi-detached factory?
Sometimes, but check three things first. The foundation must stay within your own lot at the party wall, the floor and ground must suit the machine's loads, and vibration at the neighbours must stay within the DOE's recommended limits, which are tighter for homes and shops than for factories. A detached factory with space around the press is usually easier.
Is epoxy flooring necessary for a factory?
Not by law for every factory. It is needed in effect where rules require an impervious, washable or crack-free floor, such as food premises under the Food Hygiene Regulations 2009 and scheduled waste stores under the DOE guideline, or where chemicals, static or hygiene audits demand it. For forklift traffic, choose a thicker system (FeRFA type 4 or above) rather than a thin coating.
How thick should a concrete slab be for a warehouse?
There is no standard thickness: it depends on the racking and forklift loads, the ground, the joints and whether the slab is ground-bearing or piled. Thickness alone does not tell you the capacity. Ask for the design load on the structural plans, compare it with your loads using a floor loading calculator, and have a Professional Engineer confirm.
Frequently Asked Questions
How can I tell if a factory floor has settled?
Look for floors that slope or hold water, sunken bays near doors and drains, cracks with one side lower than the other, gaps between the floor and the walls, and roller shutters that start to jam. Then confirm it: a level survey across the bays shows sunken areas, and crack gauges or tell-tale monitors read again over a few weeks show whether the movement continues. On soft ground such as parts of Klang, ask whether the slab sits on the ground or on piles, and have a Professional Engineer assess anything structural.
How much cracking is acceptable in new concrete?
There is no single legal crack width for a factory floor in Malaysia: the acceptable width is whatever the floor's design and specification allow, so ask the designer or contractor for it. ACIFC notes that a joint is essentially a planned crack and that a non-structural crack within the specified tolerances needs no repair. What matters most is whether a crack keeps opening.
What are settlement cracks in buildings?
They are cracks caused by part of a building or floor moving down more than the rest, usually because the soil or fill underneath compresses or washes out. In walls they are typically diagonal and stepped, wider at the top and running through door and window openings; in floors they show as sunken bays, stepped edges and gaps at the walls. They need monitoring and an engineer, not just filler.
How do I know if a crack in my factory floor is serious?
Look at the pattern and whether it moves. One side lower than the other, sunken areas, gaps under walls, jamming shutters or a crack that widens over weeks are warning signs, while fine shrinkage cracks that stay the same width usually are not. A crack gauge and dated photos over a few weeks give the answer, and a Professional Engineer should assess anything that looks structural.
How much does it cost to fix a crack in a concrete floor?
It varies too much for one figure. Sealing a stable shrinkage crack is minor work, while repairing settlement may need grouting, recasting or micropiles. The price depends on the cause, the area, the method and whether the factory keeps running, so get an engineer's repair scheme first and compare quotes priced on that scheme.
Can a weak factory floor be strengthened for heavy machines?
Usually yes. An engineer can recast thicker reinforced pads under the machines, refill voids under the slab, support the floor on micropiles where the ground is soft, or bond FRP strips under a suspended floor. Because this is a structural alteration, it needs a Professional Engineer's design and the council's written permission, and a tenant also needs the landlord's consent.
Can floor settlement be repaired?
Yes, once the cause is known and the movement has stopped or been stopped. Voids can be filled with grout and curled joints ground level; where the ground keeps settling, the slab or pads can be underpinned with micropiles down to firmer layers. On deep soft clay, as in parts of Klang, piled repairs need geotechnical design because settling clay drags down on piles over time.
Do I need approval to build a machine foundation or press pit?
Generally yes. A foundation or pit is building work, and section 70 of the Street, Drainage and Building Act 1974 makes altering a building without the council's prior written permission an offence; minor works may go through a simpler permit if the council agrees. In a rented factory, get the landlord's written consent and agree on reinstatement before work starts.